PERKUATAN KOLOM BULAT BETON BERTULANG DENGAN LAPIS GLASS FIBER REINFORCED POLYMER ( GFRP )
Abstract
Penelitian ini dilakukan untuk mengetahui pengaruh perkuatan kolom bulat beton bertulang dengan metode jacketing menggunakan Glass Fiber Reinforced Polymer (GFRP) dengan panjang sambungan (overlapping) GFRP yang bervariasi terhadap perilaku keruntuhan, daya dukung aksial dan daktilitas aksial kolom. Sebanyak 21 buah silinder beton dengan diameter 150 mm dan tinggi 300 mm dibuat dan dites. Variasi panjang sambungan GFRP adalah 100%, 150%, 200%, 250% dan 300% dari panjang sambungan hasil perhitungan yang didasarkan pada kuat tarik dan kuat rekatan GFRP. Pengujian dilakukan dengan memberikan beban tekan pada benda uji sampai benda uji mengalami keruntuhan. Data yang dicatat dalam pengujian adalah perilaku runtuh, beban maksimum benda uji dan perpendekan longitudinal benda uji untuk setiap peningkatan beban sebesar 10 kN. GFRP dengan sambungan 100% dan 150% mengalami gagal geser pada sambungan sedangkan GFRP dengan sambungan 200% sampai dengan 300% gagal tarik (putus) di luar sambungan. Hasil pengujian menunjukkan perkuatan kolom bulat beton bertulang dengan metode jacketing/wrapping dengan satu lapis GFRP mampu meningkatkan daya dukung aksial sebesar 11,86% sampai dengan 15,25% dan daktilitas aksial sebesar 12,41 % sampai dengan 47,14%. Abstract: The paper presents an experimental investigation the effect of circular reinforced concrete short columns strengthening using Glass Fiber Reinforced Polymer (GFRP) wrap with variation of overlapping to failure behavior, axial capacity and axial ductility. Twenty one cylindrical concrete specimens with diameters of 150 mm, and 300 mm high were made and tested. Variations of overlapping in this research were 100%, 150%, 200%, 250% and 300 % from overlapping that calculation with GFRP ultimate tension and ultimate debonding strength. Compressive load was applied to the specimens until the specimens failure. Data that note when test were; failure behavior, maximum load and longitudinal strain for every 10 kN increasing load. GFRP with overlapping 100% and 150% failed by sliding (debonding) in overlapping zone, while GFRP with overlapping 200% until 300% failed by broken outside overlapping zone. The experimental results show that circular reinforced concrete columns strengthening by jacketing method/wrapping using one layer of GFRP sheet increasing axial capacity by 11,86% until 15,25% and axial ductility by 12,41% until 47,14%.Downloads
Download data is not yet available.
How to Cite
SUDARSANA, I Ketut; GEDE SUTAPA, A.A.
PERKUATAN KOLOM BULAT BETON BERTULANG DENGAN LAPIS GLASS FIBER REINFORCED POLYMER ( GFRP ).
Jurnal Ilmiah Teknik Sipil, [S.l.], nov. 2012.
ISSN 2541-5484.
Available at: <https://ojs.unud.ac.id/index.php/jits/article/view/3455>. Date accessed: 05 nov. 2024.
Section
Articles
Keywords
perkuatan, metode jacketing, kolom bulat beton bertulang, GFRP, daya dukung aksial, daktilitas aksial.